When the tube filler machine is filling, the end of the tube is always not tightly pressed, and the material often leaks. How should this be debugged?
If the sealing of the tube filling and sealing machine is not firm, you can generally try to adjust four related parameters:
1. The temperature of the heater. Generally, the hose filling and sealing machine will have a temperature display. There are two rows of temperature. The upper row displays the heating temperature number, and the lower row displays the temperature in green. It is set by the manufacturer when it leaves the factory. It can be turned on. one operation. As shown in the figure below:
Hose Filling and Sealing Machine Temperature Display This temperature is set for hoses of different materials. It is a number determined after many attempts and cannot be changed at will.
2. The clamping pressure of the sealing splint. Generally, the clamps of the hose filling and sealing machine have a good bite and the tail is beautiful. However, when the pin of the clamp falls off, the clamps cannot bite each other, and the tail cannot be pressed normally, which will also make the soft Tube leaking. Normal embossment is as follows:
Hose filling and sealing machine Mold occlusal teeth are clear and embossed beautifully
3. Air pressure. Generally, hose filling and sealing machines need a stable air pressure, which can make the filling volume of the filling machine stable, the depth of the lettering stable, the seal is firm, and no liquid will leak. If the air pressure Instability will also appear in the picture above;
4. The speed or heating time of the hose filling and sealing machine, and the clamping time of the splint. Increasing the temperature, clamping pressure value, heating time, and clamping force can increase the fastness of the end seal. It takes many attempts to determine whether the firmness of the end seal reaches the desired number. This needs to be determined objectively, and there is no one Hard indicators;
5. Emulsion sticking to the tail of the hose filling and sealing machine will also cause the seal to be weak, and there may be liquid leakage. At this time, it is necessary to check whether the filling is normal, whether there is splashing or broken material is not straightforward, or Problems such as nozzle stickiness and filling splash are sometimes related to air pressure, which needs to be kept in mind;
6. The sealing time of aluminum-plastic pipes and all-plastic pipes is different. Aluminum-plastic pipes are much more difficult to adjust than all-plastic pipes, so don’t forget to send more packaging materials to the manufacturer when testing the machine, and let them try a lot. Often small problems are found in mass production. It is difficult to choose between the appearance and sealing strength of aluminum-plastic pipes and all-plastic pipes. Aluminum-plastic pipes cannot achieve the aesthetics of all-plastic pipes, but ensuring reliable sealing is the most important thing.
Smart Zhitong has many years of experience in the development, design tube filler machine
Please visit website for more details: https://www.cosmeticagitator.com/tubes-filling-machine/
If you have concerns please contact
Post time: Jan-12-2023